High-quality castables
THERMOcast dense castables form a solid basis for every wear-resistant refractory lining. We offer our customers a high-quality range of proven castable grades, demand-oriented and individually adapted to the respective requirements.
We stock a broad range, from inexpensive standard castables based on chamotte to high-grade ultra-low-cement castables (ULCC) based on corundum. The proven THERMOcast castables give you a high degree of flexibility with maximum process reliability and service life. Depending on the installation situation, our castables are available in different versions:
- dense refractory castable “THERMOcast”
- dense refractory gunning mix “THERMOgun”
- dense plastic ramming mix “THERMOram”
Further castable versions available on request.

Your advantages
Advantages of castables
What are the advantages of using THERMO castables in industrial furnace and plant construction:
- free choice of shape
- wide individual choice of materials
- high chemical resistance
- high mechanical strength
- good thermal shock resistance
- good heat storage
Technical data
Find your castable quickly
Here you will find an overview of some THERMOcast castables from the Thermo product range. Our table lets you make a quick preselection from the wide range of castables. Under Download you will find the technical data sheet (TDS) with the technical properties. Further grades on request. Give us a call and let us advise you!
Dense refractory castables
| THERMOcast | KT °C | RD t/m³ | KDF MPa | Chemistry (%) Al2O3 | Chemistry (%) CaO | Chemistry (%) Fe2O3 | Technical data sheet |
|---|---|---|---|---|---|---|---|
| THERMOcast 1300S | 1300 | 2,1 | 75 | 38,5 | 3,4 | 2,2 | Download |
| THERMOcast 1480 AR/R/TS | 1500 | 2,4 | 130 | 50,0 | 2,5 | 0,8 | Download |
| THERMOcast 1521 | 1550 | 2,3 | 70 | 52,2 | 1,8 | 0,6 | Download |
| THERMOcast 1640S | 1640 | 2,6 | 70 | 66,4 | 1,5 | 0,8 | Download |
| THERMOcast 1650S | 1650 | 2,5 | 90 | 60,0 | 2,3 | 1,0 | Download |
| THERMOcast 1820 C/R | 1820 | 2,6 | 80 | 95,0 | 4,4 | 0,1 | Download |
| THERMOflow 1480 AR/R/TS | 1500 | 2,3 | 80 | 50,0 | 2,5 | 0,8 | Download |
| KT = classification temperature | RD = bulk density | KDF = cold crushing strength 110°C | WLF = thermal conductivity | |||||||
| THERMOgun | KT °C | RD t/m³ | KDF MPa | Chemistry (%) Al2O3 | Chemistry (%) CaO | Chemistry (%) Fe2O3 | Technical data sheet |
|---|---|---|---|---|---|---|---|
| THERMOgun 1300S | 1400 | 1,96 | 35 | 40,2 | 7,7 | 4,4 | Download |
| THERMOgun 1453 | 1550 | 2,1 | 70 | 54,5 | 6,5 | 0,6 | Download |
| THERMOgun 1480 AR/R/TS | 1500 | 2,1 | 50 | 40,0 | 2,7 | 0,9 | Download |
| THERMOgun 1600S | 1600 | 2,5 | 50 | 60,2 | 2,4 | 0,9 | Download |
| THERMOgun 1650S | 1650 | 2,3 | 15 | 79,2 | 4,3 | 1,6 | Download |
| THERMOgun 1700S | 1700 | 2,5 | 45 | 93,2 | 5,8 | 0,2 | Download |
| KT = classification temperature | RD = bulk density | KDF = cold crushing strength 110°C | WLF = thermal conductivity | |||||||